Skip to main content

Welding Gas Regulator Settings Guide: MIG, TIG & Oxy-Acetylene Pressure Charts

Welding Gas Regulator Settings Guide MIG, TIG & Oxy-Acetylene Pressure Charts

Getting your regulator pressure and flow rate right is one of the simplest ways to improve weld quality, reduce gas waste, and avoid common problems like porosity, burn-through, and excessive spatter. Yet it’s one of the most frequently asked questions we get from welders — especially those setting up a new process or working with unfamiliar material.

Here are the recommended settings for the most common welding processes used in Melbourne workshops.

MIG Welding (GMAW) — Flow Rate Settings

MIG welding uses a constant flow of shielding gas measured in litres per minute (L/min). The flow rate depends on your nozzle size, wire diameter, and working conditions.

General mild steel (Argon/CO2 mix — 75/25 or 80/20):

0.6mm wire: 8–10 L/min

0.8mm wire: 10–12 L/min

0.9mm wire: 12–14 L/min

1.2mm wire: 14–18 L/min

Pure CO2 (mild steel, deeper penetration):

Same flow rates as above, but you may need to increase by 1–2 L/min due to CO2’s higher thermal conductivity and tendency to create more turbulence at the arc.

Aluminium (pure argon):

1.0mm wire: 14–16 L/min

1.2mm wire: 16–20 L/min

Aluminium is more sensitive to contamination, so slightly higher flow rates help ensure good coverage.

Stainless steel (Argon + 2% CO2 or tri-mix):

0.8mm wire: 10–12 L/min

0.9mm wire: 12–14 L/min

TIG Welding (GTAW) — Flow Rate Settings

TIG uses pure argon (or argon/helium mix for thicker aluminium). Flow rates are generally lower than MIG because the gas cup provides more focused coverage.

Standard TIG (pure argon):

Cup size #5 (8mm): 5–7 L/min

Cup size #6 (10mm): 6–8 L/min

Cup size #7 (11mm): 7–10 L/min

Cup size #8 (13mm): 8–12 L/min

Large gas lens cups (#12+): 12–18 L/min

Aluminium TIG (argon or argon/helium):

Use the same cup-based flow rates above. If using an argon/helium mix, increase flow by 10–15% — helium is lighter and dissipates faster.

Post-flow: Set your post-flow timer to at least 5–8 seconds. This keeps shielding gas flowing after the arc stops, protecting the cooling weld pool and tungsten from oxidation. For aluminium and stainless, use 8–12 seconds.

Oxy-Acetylene — Pressure Settings

Oxy-acetylene uses pressure (measured in kPa or PSI) rather than flow rate. Getting the balance between oxygen and acetylene right is critical for a clean, stable flame.

Cutting (oxy-acetylene):

Material up to 12mm: Oxygen 200–250 kPa (30–35 PSI), Acetylene 55–70 kPa (8–10 PSI)

Material 12–25mm: Oxygen 250–300 kPa (35–45 PSI), Acetylene 55–70 kPa (8–10 PSI)

Material 25–50mm: Oxygen 300–400 kPa (45–60 PSI), Acetylene 55–70 kPa (8–10 PSI)

CRITICAL SAFETY NOTE: Never exceed 103 kPa (15 PSI) on the acetylene regulator. Above this pressure, acetylene becomes unstable and can decompose explosively. This is a hard limit that applies to all acetylene use, regardless of application.

Welding (oxy-acetylene):

Thin material (1–3mm): Oxygen 15–30 kPa, Acetylene 15–30 kPa

Medium material (3–6mm): Oxygen 30–50 kPa, Acetylene 30–50 kPa

Adjust tip size to match material thickness — pressure alone won’t compensate for a wrong tip.

Brazing:

Oxygen 15–30 kPa, Acetylene 15–30 kPa. Use a slightly carburising (excess acetylene) flame for brazing — the inner cone should have a slight feather.

Common Problems and What They Mean

Porosity (tiny holes in the weld): Usually means insufficient shielding gas. Increase your flow rate by 2–3 L/min. Also check for drafts — wind as low as 5 km/h can disrupt gas coverage. If you’re welding outdoors, use a windbreak or increase flow by 20–30%.

Excessive spatter: On MIG, this often means your flow rate is too high, creating turbulence that draws air into the shielding gas stream. More gas isn’t always better — try reducing flow by 2 L/min.

Black or oxidised welds (TIG): Insufficient gas coverage. Increase flow rate, check for leaks in your torch, or use a larger cup. On stainless steel, also check your post-flow time — if the weld is discolouring as it cools, post-flow is too short.

Burn-through on thin material: Not a gas problem — reduce your amperage or increase travel speed. But ensuring proper gas coverage prevents oxidation that can make thin material more prone to burning through.

Irregular oxy-acetylene flame: Dirty tip, incorrect pressures, or a blocked mixer. Clean the tip with proper tip cleaners (not a wire brush), check both regulator settings, and ensure your flashback arrestors aren’t tripped.

Tips for Reducing Gas Waste

Don’t set and forget: Adjust your flow rate for each job. Running 18 L/min on thin sheet metal when 10 would do is just burning money.

Check for leaks regularly: A slow leak at a fitting can empty a cylinder over a weekend. Use soapy water on all connections periodically.

Use the right regulator: A regulator designed for high-flow industrial use gives more consistent output than a cheap hobby regulator. It pays for itself in gas savings.

Pre-flow and post-flow: On TIG, set pre-flow to 0.5–1 second and post-flow to 5–12 seconds. This uses a small amount of gas but prevents contamination that would mean grinding out and re-doing the weld — which wastes far more gas.

Related Services

 

Call 1300 733 097

Request a Quote

Puregas Australia Gas Supplier
Gas supply. Done right.
Australian-owned gas supply for industrial, welding, hospitality, food-grade, LPG and specialist supply needs.

Clear terms. Straight pricing. Specialist gas advice. One number.
Welding, hospitality and selected cylinder gases available nationally through 200+ dealer locations. Specialist supply confirmed by location.
One number · Orders · Trade accounts · Technical & SDS · Wholesale.
Melbourne operations
Victoria, Australia
Mon–Fri 8–4:30
© 2026 Puregas Pty Ltd. All rights reserved.